Quality6 min read

Colourfastness Tests for Hotel Rugs Explained

The three colourfastness tests that matter for hotel rugs, light, rubbing and water, how ISO 105 grades them, and how to write them into a spec.

EM

Eastern Mills Editorial

Eastern Mills

Colourfastness Tests for Hotel Rugs Explained

For hotel rugs, three colourfastness tests matter most: fastness to light, which predicts fading near windows; fastness to rubbing, which predicts colour transferring onto shoes, luggage and adjacent floors; and fastness to water, which predicts bleeding when the rug is spilled on or wet cleaned. Each is measured by a method in the ISO 105 series, or its AATCC equivalent in the United States, and graded on a numbered scale where a higher number means a better result.

Why hotels are hard on colour

A residential rug might be cleaned professionally once a year. A hotel rug is vacuumed daily, spot cleaned often, extracted regularly and sometimes sits in strong sun through a full height window for years. Spills are frequent and housekeeping chemicals vary. A colour that is acceptable at home can fail within one refurbishment cycle in a hotel.

Colourfastness testing gives a measurable result before bulk production, so that these failures are found on a sample rather than on the guest floor.

The three tests

PropertyISO methodCommon US methodWhat it simulatesHow it is graded
LightISO 105-B02, xenon arc lampAATCC TM16.3Fading under daylight through glassAgainst blue wool references, 1 to 8
RubbingISO 105-X12, dry and wetAATCC TM8Colour transferring to anything that rubs the pileStaining of a white rubbing cloth, grey scale 1 to 5
WaterISO 105-E01AATCC TM107Bleeding when the rug is wetChange in the specimen and staining of adjacent fabrics, grey scale 1 to 5

The scales are not the same. Light fastness under ISO 105-B02 is rated by comparison with blue wool references, numbered 1 to 8 in the European set, or L2 to L9 in the set more often used in America. The standard notes that results from the two sets are not interchangeable. Rubbing and water results are rated with grey scales: ISO 105-A02 for change in colour and ISO 105-A03 for staining. Each grey scale has five steps, and augmented scales add half steps such as 4 to 5 and 3 to 4.

A grade 5 on a grey scale means no visible change or staining. A grade 1 means severe change or staining.

Light fastness in practice

Fading depends on the dye, the fibre, the depth of shade and the exposure. Pale shades of some colours fade more visibly than deep shades. Lobbies with glazed facades, guest rooms with large south facing windows in the northern hemisphere, and resort interiors with open terraces are the highest risk.

Practical steps:

  • Identify rugs that will sit in direct sun and require light fastness testing for those colours.
  • Ask for light fastness results on the actual colours, not on a representative shade.
  • Specify light fastness on the blue wool scale used by the laboratory and state which set.
  • Consider window films, blinds and rug rotation in the operating plan for the brightest positions.

Rubbing fastness in practice

Rubbing is tested both dry and wet, because wet rubbing usually transfers more colour. Deep shades, especially dark reds, navies and blacks, are the usual weak point. A rug that rubs off can stain light stone at its edges, the wheels of luggage and housekeeping cloths.

Ask for both dry and wet results for every deep shade in the design. If a colour is borderline, the dyer may adjust the recipe, the dye class or the after treatment, or the designer may choose a slightly different shade.

Water fastness in practice

Hotels spot clean and wet extract. A colour that bleeds will migrate into neighbouring light colours, which is most visible in high contrast designs such as a navy motif on an ivory ground. The water test shows both whether the dyed yarn changes and whether it stains adjacent undyed fibres.

High contrast designs and designs with large ivory or white areas deserve water fastness testing on every dark colour that touches a light one.

Fibre and dye choices that affect results

  • Wool takes acid and metal complex dyes well and is the fibre most used in hotel rugs.
  • Viscose and other regenerated cellulose fibres use different dye classes and are more sensitive to water.
  • Silk accents behave differently again and are best kept away from heavy wet cleaning.
  • Undyed natural wool removes the dye question entirely for those areas.

A rug with several fibres should be tested for each fibre and colour combination that matters, not only the ground.

Writing it into the specification

ItemWhat to state
MethodsISO 105-B02, ISO 105-X12 dry and wet, ISO 105-E01, or the AATCC methods for a US project
Minimum gradesOne minimum for each test, set by the brand standard or the design team
ScopeWhich colours and fibres are tested, for example every deep shade and every colour adjacent to ivory
LaboratoryIndependent and accredited for the methods, or the manufacturer's laboratory with independent verification
TimingResults approved with the strike-off, before bulk
Lot controlWhether a production lot is retested

How Eastern Mills approaches colourfastness

Eastern Mills spins and dyes yarn in house at its site in Bhadohi, and works to colourfastness of Grade 4 to 5 to ISO 105. Where a project names particular methods, grades or laboratories, testing to that standard is arranged per order on the yarn and construction to be supplied. Dyeing, weaving and finishing on one site is described on our manufacturing infrastructure page, and yarn production on the spinning page. To discuss a colour programme, contact us.

Frequently asked questions

What is a good rubbing fastness grade for hotel rugs?

Grades are set by the brand standard or the design team. Specify a minimum for dry and for wet rubbing separately, since wet results are usually lower.

Is light fastness graded the same way as rubbing?

No. Light is graded against blue wool references on a scale of 1 to 8 or L2 to L9, while rubbing and water use grey scales of 1 to 5.

Do natural dyes perform better?

Not necessarily. Natural dyes vary widely in light and water fastness. Test the actual colours.

Does washing in finishing affect the result?

Yes. Washing removes loose dye and can improve rubbing and water results. Tests should be made on finished, washed samples.

Posted in:Quality